2507 Duplex Stainless Steel Bar

2507 duplex stainless steel bar is made of a special ferritic-austenitic duplex stainless steel featuring excellent corrosion resistance. It performs comprehensive protection against point corrosion, crevice corrosion and uniform corrosion through the ratio of chromium and molybdenum elements.

Guaranteed Safe Checkout

2507 Duplex Stainless Steel Bar Description

2507 duplex stainless steel bar is made of an ultra-duplex stainless steel containing 25% chromium, 4% molybdenum and 7% nickel. In terms of chemical composition, 2507 stainless steel has relatively high content of chromium and molybdenum, which accounts for its strong corrosion resistance to various acids. Besides, it has excellent resistance to stress corrosion cracking owing to the duplex construction of 2507 stainless steel. 2507 stainless steel bars show excellent corrosion resistance in environments containing chloride ions, which makes it ideal for construction and related industries. In addition, 2507 stainless steel also has excellent mechanical properties including high compressive strength, impact strength and low coefficient of thermal expansion. So 2507 duplex stainless steel bars are widely adopted as manufacturing parts in fields including oil and gas, water treatment, fire protection, desalination equipment, mechanical parts and fuel gas purification equipment.

Product Parameters

Product Name 2507 Duplex Stainless Steel Bar
Type Steel Bar
Outer Diameter Round Bar 4mm-500mm
Hexagon Bar 18mm-57mm (11/16″ to 2-3/4″)
Square Bar 18mm-47mm (11/16″ to 1-3/4″)
Flat Steel 1/2 “to 10”, Thickness: 2mm-150mm, Can provide customized
Length 1-6 meters, Length can be customized
Standard ASTM, AISI, JIS, GB, DIN, EN, etc.
Surface Black, Bright Polished, Rough Turning, Mattness Surface Treatment, No. 4. BA, etc.
Scope of Application Stainless steel bars are used in a variety of industries such as shipbuilding,

Defense, Automotive, Textiles, Paper and pulp, Manufacturing, Cement,

Heavy earthmoving equipment and construction, etc.

Chemical Composition

C Si Mn Cr Ni Mo S P
≤ 0.03 ≤ 0.8 ≤ 1.2 24.0~26.0 6.0~8.0 3.0~5.0 ≤ 0.02 ≤ 0.035

Mechanical Properties

Tensile Strength Kb (MPa) Yield Strength σ0.2 (MPa) Elongation D5 (%) Hardness
≥795 ≥550 ≥15 ≤ 310HB

Physical Performance

Density(g/cm³) Modulus of Elasticity(Gpa) Coefficient of Thermal Expansion(10-6/°C) Coefficient of Thermal Conductivity(W/m*K) Resistivity(ΜΩ. cm)
7.75 200 13.0 17.0 80